Hello leatherworkers
I have for the last year or so been using the Eco-Flo Professional Finishes and have had great results. I have just brought some Eco-Flo (standard) Finish and I am am not getting the same result. Before I was getting a nice smooth clear finish but now I am left with a poor finish that has a kind of white powdery finish.
I am currently using the Eco-Flo water based dyes and find the colours good and have had no problems with the dye coming out even after several year heavy use. I have this week also brought some Fibbing's oil dyes and plan on testing these.
My main question is can anyone suggest a good proofer/fisishing product that will work well with Eco-Flo water based dyes and Fibbing's oil dyes? I am making wallets, notebook cases, keychain ect.
Also if anyone suggest a good proofer/fisishing product that will work well with tannery dyed leather? I am making handbag/satchels.
Thanks for you Help.