Members LederRudi Posted November 14, 2013 Members Report Posted November 14, 2013 Hi all, what kind of finish would you recommend after the application of Fiebing’s Professional Oil Dye? Quote
Members Dwight Posted November 14, 2013 Members Report Posted November 14, 2013 Most of my leather items are belts, holsters, wallets, knife sheaths, magazine carriers, and a very occasional wallet or purse. I use Feibings oil dye on almost all of them. I use Resolene as the final finish, again, on almost all of them. The exception is usually a period piece, deemed to look like it is much older, . . . on it I will use a blend of beeswax and neatsfoot oil. The Resolene is always mixed with water in a 50/50 concentration, . . . applied with a cheap little bristle brush. Hope this helps. May God bless, Dwight Quote
Members LederRudi Posted November 14, 2013 Author Members Report Posted November 14, 2013 Thank you, Dwight! Quote
Members nrk Posted November 25, 2013 Members Report Posted November 25, 2013 Most of my leather items are belts, holsters, wallets, knife sheaths, magazine carriers, and a very occasional wallet or purse. I use Feibings oil dye on almost all of them. I use Resolene as the final finish, again, on almost all of them. The exception is usually a period piece, deemed to look like it is much older, . . . on it I will use a blend of beeswax and neatsfoot oil. The Resolene is always mixed with water in a 50/50 concentration, . . . applied with a cheap little bristle brush. Hope this helps. May God bless, Dwight Hi, what is the reason of mixing Resolene with water?? Quote
Members Cyberthrasher Posted November 25, 2013 Members Report Posted November 25, 2013 Hi, what is the reason of mixing Resolene with water?? because if you don't, it will ALWAYS apply to heavily with an extreme amount of gloss and the possibility of cracking, and that's if you manage to get it on cleanly without any smears and bubbles. Always apply it 50/50, building up your desired coverage with light coats. Quote
Members nrk Posted November 26, 2013 Members Report Posted November 26, 2013 because if you don't, it will ALWAYS apply to heavily with an extreme amount of gloss and the possibility of cracking, and that's if you manage to get it on cleanly without any smears and bubbles. Always apply it 50/50, building up your desired coverage with light coats. Copied that. Thanx for the tip. Quote
Chief31794 Posted November 26, 2013 Report Posted November 26, 2013 because if you don't, it will ALWAYS apply to heavily with an extreme amount of gloss and the possibility of cracking, and that's if you manage to get it on cleanly without any smears and bubbles. Always apply it 50/50, building up your desired coverage with light coats. Totally on the mark, I use TanKote as well and cut it 50/50 with distilled water. Both are too concentrated in their purchased form in my opinion. Not to mention that you get twice as much finish. Chief Quote
Members nrk Posted November 27, 2013 Members Report Posted November 27, 2013 Totally on the mark, I use TanKote as well and cut it 50/50 with distilled water. Both are too concentrated in their purchased form in my opinion. Not to mention that you get twice as much finish. Chief Truth is yours. Agree. N Quote
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.